Aleazio mota / Errendimendua | 1Cr13Al4 | 0Cr25Al5 | 0Cr21Al6 | 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
Konposizioa | Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 | 20,5-23,5 | 18.0-21.0 | 21.0-23.0 | 26,5-27,8 |
Al | 4,0-6,0 | 4,5-6,5 | 5,0-7,0 | 4.2-5.3 | 3.0-4.2 | 5,0-7,0 | 6,0-7,0 | |
Re | Aukerakoa | |||||||
Fe | Atseden | |||||||
Nb0.5 | Mo1.8-2.2 | |||||||
Max. etengabeko zerbitzuaren tenperatura. elementuaren (℃) | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
Erresistentzia 20 ℃ (μm.m) | 1.25 | 1.42 | 1.42 | 1.35 | 1.23 | 1.45 | 1.53 | |
Dentsitatea (g/cm3) | 7.4 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 | |
Eroankortasun termikoa (KJ/mh ℃) | 52.7 | 46.1 | 63.2 | 60.2 | 46.9 | 46.1 | – | |
Lerroen hedapen koefizientea (ax10-6/℃) | 15.4 | 16 | 14.7 | 15 | 13.5 | 16 | 16 | |
Urtze-puntua gutxi gorabehera (℃) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
Gogortasuna (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
Luzapena hausturan (%) | > 16 | > 12 | > 12 | > 12 | > 12 | > 12 | > 10 | |
Errepikatu tolestura-maiztasuna (F/R) | > 5 | > 5 | > 5 | > 5 | > 5 | > 5 | > 5 | |
Etengabeko zerbitzu-denbora (orduak/℃) | – | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥80/1350 | ≥80/1350 | |
Trakzio erresistentzia (N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 650-800 | |
Eremuaren aldakuntza (%) | 65-75 | 60-75 | 60-75 | 60-75 | 60-75 | 60-75 | 60-75 | |
Egitura mikrografikoa | Ferrita | Ferrita | Ferrita | Ferrita | Ferrita | Ferrita | Ferrita | |
Propietate magnetikoak | Magnetikoa | Magnetikoa | Magnetikoa | Magnetikoa | Magnetikoa | Magnetikoa | Magnetikoa |